Tensile Test Laboratory Report

Tensile Test Laboratory Report
Introduction
In mechanical testing, one of the common properties widely used is the strength of materials. In this lab report, tensile testing was used to determine these strengths. The experiment provides details on the mechanical behavior or strength of a material. The foundational idea is to place the material specimen between fixtures known as grips which clamp the specimens. For comparison purposes, these materials should have equal dimensions of initial measurements such as lengths, and cross-sectional areas (Callister & Rethwisch, 2007). After confirming these dimensions, we can then begin to apply the loads or forces or weights while at the same time recording the change in lengths as the weights are steadily increased.
A very simple test requires one to hang some materials on an immovable grip and the weights on hooked end. To ensure the change in the consecutive lengths, add the weights to keep the material to stretch until the point of breakage. The experiment gives a result of a graph of force (N) against extension (mm), and because the force required in stretching the materials depends on the strength of the materials, a comparison between the specimens can be easily obtained. The various abilities of the materials can be very crucial to a structural designer who must ensure that the materials withstand certain forces. This mechanical strengths and behavioral properties of materials can only be found when these materials are tested and pulled until breakage. In this experiment, the three materials which were brass, aluminum, steel and stainless steel were used as specimens. The strength properties were used to determine their tensile strengths and Young’s modulus.
Objectives
The experiment is to examine the behavior of four material specimens under the tensile test. The materials under the test are brass, steel, aluminum and stainless steel. From the tensile test, the properties that will be determined are the tensile strengths, 0.2% proof stress and Young’s modulus (Yoshida, Uemori & Fujiwara, 2002). This experiment is used to establish materials properties. Moreover, it can be used in diverse industries. An example where the tensile test can be applied is to decide the Ultimate Tensile Stress required for building structures, railways, shopping bags, et cetera (Hosford & Caddell, 2011).
Equipment and Methodology
Four composite specimens of brass, stainless steel, steel, and aluminum, and which have equal dimensions. The test was performed by putting the specimens under a test machine that contain grips to hold the specimens (Meyers & Chawla, 2009). The machine then was allowed to exert tensile forces, causing the specimen to extend. As was read from the machine, the load per increment and the specimen extensions were written down for analysis. The loads and lengths of all the materials were recorded and then compared with each other.
Results and Analyses

Load (N)-Extension (mm) Curve for Brass, Stainless steel, steel, and Aluminum

Calculations
Given the materials with equal dimensions, in this experiments case 10mm diameter and 60mm material length. We can perform the following calculations;
Tensile strength = (Maximum Load)/(Cross Sectional Area)
At the maximum load of 7665N, Stainless Steel Yields a tensile strength of
Tensile strength = 7665/78.57
= 97.55 N/mm2 Or 0.098kN/mm2
At the maximum load of 3769N, Brass Yields a tensile strength of
Tensile strength = 3769/78.57
= 47.97 N/mm2 Or 0.048kN/mm2
At the maximum load of 3652N, Steel Yields a tensile strength of
Tensile strength = 3652/78.57
= 46.48 N/mm2 Or 0.04648kN/mm2
At the maximum load of 811N, Aluminum Yields a tensile strength of
Tensile strength = 811/78.57
= 10.322 N/mm2 Or 0.0103kN/mm2
The Proof Stress at 0.2% of these materials can be calculated as follows;
0.2% of 60mm is equal to 12mm. Therefore, at 12 mm, by reading this value against the corresponding load, we get the proof load of Stainless steel as 0.06216kN, Brass as 0.034kN, and Steel as 0.03350kN. The aluminum breaks before attaining the 0.2% proof Load.
The 0.2% proof Stress is therefore given as;
Stainless Steel, Proof Load = 0.0621kN/78.57mm2
Proof Load= 0.00079kN/mm2
Brass, Proof Load = 0.034kN/78.57mm2
Proof Load= 0.000433kN/mm2
Steel, Proof Load = 0.0335kN/78.57mm2
Proof Load= 0.000424kN/mm2
Young’s Modulus
From an elastic curve region in the diagram, we can obtain Young’s Modulus (Chen, Gandhi, Lee, & Wagoner, 2016).
In stainless Steel experiment, Young^’ s Modulus = Stress/Strain
Stress= Load/(Cross Sectional Area)
Strain= Extension/(Original Length)
For Stainless Steel,
Stress= 3.384kN/78.57mm2
Strain= 0.3mm/60mm
Young^’ s Modulus = 0.04307/0.005
Young^’ s Modulus = 8.614kN/mm2
For Brass,
Stress= 2.168kN/78.57mm2
Strain= 0.3mm/60mm
Young^’ s Modulus = 5.519kN/mm2
For Steel,
Stress= 1.318kN/78.57mm2
Strain= 0.17mm/60mm
Young^’ s Modulus = 0.01677/0.002833
Young^’ s Modulus = 5.92kN/mm2

For Aluminum,
Stress= 0.569kN/78.57mm2
Strain= 0.17mm/60mm
Young^’ s Modulus = 0.00724/0.002833
Young^’ s Modulus = 2.56kN/mm2
Discussions
These graphical analyses were conducted from the data that was obtained from the specimens after the experimentations. From the load-extension curves, the tensile strengths, 0.2% proof stress and Young’s modulus for the four specimens are as calculated below.
The first phase of each graph is the elastic region. This is where the specimens extend uniformly with the load added. The second stage when the curve begins to bend is known as the offset yield strength; in this lab, calculated at 0.2%. After the materials extend up to the maximum reachable stress, they fail to hold any more loads and; therefore, break. This point of breakage is known as the Fracture point. The elasticity limits of brass, stainless steel, steel, and aluminum differ with their respective tensile strengths obtained from the calculations. From our analysis, stainless steel is found to have the highest tensile strength, followed by the brass, steel and finally the aluminum is the weakest (Ross, Irvin, & Roth, 2007). This means that in structural engineering, stainless steel can be the most preferred where stronger tensile forces are needed.
Conclusion
The tensile tests on stainless steel, brass, steel, and aluminum identify stainless steel to be having the highest tensile strength followed by brass, steel and finally aluminum in the above order. These results also mean that the structures made from these materials have the ability to carry heavy loads in that order starting from the stainless steel, the strongest material. By knowing the strengths of particular materials, an engineer is able to identify their suitability in coming up with rails, buildings, shopping bags and other structures. To avoid fractures and breakages, the carrying capacity of these materials must not be surpassed (Callister & Rethwisch, 2007).
References
Callister, W. D., & Rethwisch, D. G. (2007). Materials science and engineering: an introduction (Vol. 7, pp. 665-715). New York: Wiley.
Chen, Z., Gandhi, U., Lee, J., & Wagoner, R. H. (2016). Variation and consistency of Young’s modulus in steel. Journal of Materials Processing Technology, 227, 227-243.
Hosford, W. F., & Caddell, R. M. (2011). Metal forming: mechanics and metallurgy. Cambridge University Press.
Meyers, M. A., & Chawla, K. K. (2009). Mechanical behavior of materials (Vol. 2, pp. 420-425). Cambridge: Cambridge university press.
Ross, C. D., Irvin, D. B., & Roth, J. T. (2007). Manufacturing aspects relating to the effects of direct current on the tensile properties of metals. Journal of engineering materials and technology, 129(2), 342-347.
Yoshida, F., Uemori, T., & Fujiwara, K. (2002). Elastic–plastic behavior of steel sheets under in-plane cyclic tension–compression at large strain. International Journal of Plasticity, 18(5), 633-659.

Order | Check Discount

Tags: Best Assignment Help Australia, Can Someone Write My Assignment for Me, can you write my dissertation, Do my assignment Australia, do my dissertation

Assignment Help For You!

Special Offer! Get 15-30% Off on Each Order!

Why Seek Our Custom Writing Services

Every Student Wants Quality and That’s What We Deliver

Graduate Essay Writers

Only the most qualified writers are selected to be a part of our research and editorial team, with each possessing specialized knowledge in specific subjects and a background in academic writing.

Affordable Prices

Our prices strike the perfect balance between affordability and quality. We offer student-friendly rates that are competitive within the industry, without compromising on our high writing service standards.

100% Plagiarism-Free

No AI/chatgpt use. We write all our papers from scratch thus 0% similarity index. We scan every final draft before submitting it to a customer.

How it works

When you decide to place an order with Nursing.StudyBay, here is what happens:

Fill the Order Form

You will complete our order form, filling in all of the fields and giving us as much guidelines - instruction details as possible.

Assignment of Writer

We assess your order and pair it with a skilled writer who possesses the specific qualifications for that subject. They then start the research/writing from scratch.

Order in Progress and Delivery

You and the assigned expert writer have direct communication throughout the process. Upon receiving the final draft, you can either approve it or request revisions.

Giving us Feedback (and other options)

We seek to understand your experience. You can also review testimonials from other clients, from where you can select your preferred professional writer to assist with your homework assignments.

Expert paper writers are just a few clicks away

Place an order in 3 easy steps. Takes less than 5 mins.

Calculate the price of your order

You will get a personal manager and a discount.
We'll send you the first draft for approval by at
Total price:
$0.00